Color/Appearance: Heartwood color is variable, ranging from a very pale pink to a deeper reddish brown, sometimes with streaks of medium to dark reddish brown. Color tends to darken with age. Quartersawn surfaces can also exhibit a ribbon-stripe appearance.

Grain/Texture: Grain is straight to interlocked, with a medium to coarse texture. Good natural luster with a light-refracting optical phenomenon known as chatoyancy. (See video below.)

Categories: ,

Description

Specification:

Common Name(s): African Mahogany

Scientific Name: Khaya spp. (Khaya anthotheca, K. grandifoliola, K. ivorensis, K. senegalensis)

Distribution: West tropical Africa

Tree Size: 100-130 ft (30-40 m) tall, 3-5 ft (1-1.5 m) trunk diameter

Average Dried Weight: 40 lbs/ft3 (640 kg/m3)

Specific Gravity (Basic, 12% MC): .52, .64

Janka Hardness: 1,070 lbf (4,760 N)

Modulus of Rupture: 13,190 lbf/in2 (91.0 MPa)

Elastic Modulus: 1,537,000 lbf/in2 (10.60 GPa)

Crushing Strength: 7,100 lbf/in2 (49.0 MPa)

Shrinkage: Radial: 4.2%, Tangential: 5.7%, Volumetric: 10.0%, T/R Ratio: 1.4